Specializing in Tooth By Tooth Induction Hardening
Material Weight Conversions
|
Multiply the weight in steel by the listed factor for
the selected material. |
|
|
|
Material |
Conversion
Factor |
|
Material |
Conversion
Factor |
| Aluminum |
.3462 |
|
Lead |
1.448 |
| 1100 Aluminum |
.3462 |
|
Silver |
1.339 |
| 2011 Aluminum |
.3604 |
|
Molybdenum |
1.303 |
| 2014 Aluminum |
.3568 |
|
Copper |
1.144 |
| 2017 Aluminum |
.3568 |
|
Nickel |
1.137 |
| 2024 Aluminum |
.3568 |
|
Columbium |
1.095 |
| 3003 Aluminum |
.3498 |
|
Brass |
1.084 |
| 5005 Aluminum |
.3462 |
|
Monel |
1.084 |
| 5052 Aluminum |
.3427 |
|
300 Series Stainless |
1.01 |
| 5056 Aluminum |
.3356 |
|
400 Series Stainless |
1.00 |
| 5083 Aluminum |
.3392 |
|
Tin |
.932 |
| 5086 Aluminum |
.3392 |
|
Zinc |
.911 |
| 6061 Aluminum |
.3462 |
|
Cast Iron |
.911 |
| 6063 Aluminum |
.3427 |
|
Zirconium |
.812 |
| 7075 Aluminum |
.3568 |
|
Titanium |
.575 |
| 7178 Aluminum |
.3604 |
|
Beryllium |
.236 |
| Gold |
2.466 |
|
Magnesium |
.229 |
| Tungsten |
2.462 |
|
|
|
| Tantalum |
2.120 |
|
|
|



| Home
| | Process ||Capability
| | History || Quality ||
Rush |
| Contact | | Misc |
This site is best
viewed with Internet Explorer 5+ 800 X 600 Resolution
All Rights Reserved © 2003 American Metal Treating
Site Design By
Res Com Service Net
|